Alloy 909 / UNS N19909

Standards

Mat. No.
-
EU
-
AISI/ASTM
-
UNS
N19909
Other
Incoloy 909
Alloy 909
2.4711 kobalt-krom-nikel-molibden alaşımıdır.
It exhibits excellent formability, high strength, corrosion resistance, and high fatigue resistance during processing. Additionally, its strength can be increased by up to 25% through cold working. It is resistant to stress corrosion cracking. °It can perform well in temperatures ranging from cryogenic temperatures to 454°C.

Chemical Composition & Mechanical and Physical Properties

C%
0.06 max
Fe%
Rest
Ni%
35.00-40.00
Co %
12.00-16.00
Si%
0.25-0.50
Al %
0.15 max
Nb %
4.30-5.20
Ti %
1.30-1.80
Tensile Strength (1000 hours)
540 °C
900 MPa
Co%
39.00-41.00
595 °C
590 MPa
650 °C
310 MPa
0.2 %Yield Strength Rp N/mm2
1034
Tensile Strength Rm N/mm2
1276
Elongation A5 %
15 min
Precipitation hardened

Application areas

In gas turbines, rocket engines, steam turbine bolts, glass sealing.